Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CALIBRE™ MEGARAD™ 2081-15 - PC - Trinseo

Material Data Center offers the following functions for CALIBRE™ MEGARAD™ 2081-15:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Calibre Megarad datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 15 g/10min ISO 1133
温度 300 °C -
荷重 1.2 kg -
成形収縮率, 平行 0.6 % ISO 294-4, 2577
ASTM数据
メルトフローレイト, MFI 15 g/10min ASTM D 1238
温度 300 °C -
荷重 1.2 kg -
成形収縮率., 平行 0.006 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
引張弾性率 2300 MPa ISO 527
降伏応力 62 MPa ISO 527
降伏ひずみ 6 % ISO 527
破壊応力 68 MPa ISO 527
破壊ひずみ 130 % ISO 527
曲げ弾性率, 23°C 2400 MPa ISO 178
曲げ強さ 97 MPa ISO 178
ノッチ付きシャルピー衝撃強さ, +23°C 25 kJ/m² ISO 179/1eA
ノッチ付きIzod衝撃強さ, +23°C 75 kJ/m² ISO 180/1A
ASTM数据
引張弾性率 2206 MPa ASTM D 638
降伏応力 62.1 MPa ASTM D 638
破壊応力 68.3 MPa ASTM D 638
降伏点伸び 6 % ASTM D 638
破断伸び 130 % ASTM D 638
曲げ弾性率 2413 MPa ASTM D 790
曲げ強さ 96.5 MPa ASTM D 790
ロックウェル硬度 R 118 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 747 J/m ASTM D 256
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 120 °C ISO 75-1/-2
ビカット軟化温度, B 138 °C ISO 306
ASTM数据
線膨張係数, 平行 68.4 E-6/K ASTM D 696
DTUL @ 66 psi 139[ann.] °C ASTM D 648
DTUL @ 264 psi 122 °C ASTM D 648
ビカット軟化温度 143 °C ASTM D 1525
ann.: annealed
電気的特性.単位テスト基準
ISO データ
耐電圧 17 kV/mm IEC 60243-1
ASTM数据
耐電圧, 短い時間 16.5 kV/mm ASTM D 149
誘電正接, 1 MHz 0.002 - ASTM D 150
比誘電率, 60 Hz 3 - ASTM D 150
比誘電率, 1 MHz 3 - ASTM D 150
体積抵抗率 2E17 Ohm*cm ASTM D 257
光学特性単位テスト基準
ASTM数据
ヘイズ 2 % ASTM D 1003
視感透過率 85 % ASTM D 1003
くっせつりつ 1.59 - ASTM D 542
その他の特性.単位テスト基準
吸水率. 0.12 % Sim. to ISO 62
吸湿率 0.15 % Sim. to ISO 62
密度. 1200 kg/m³ ISO 1183
吸水率, 24hr 0.15 % ASTM D 570
密度 1200 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 120 °C -
Pre-drying - Time 4 h -
樹脂温度 275 - 295 °C -
金型温度 70 - 90 °C -
機能
 粘度せん断速度. , CALIBRE™ MEGARAD™ 2081-15, PC, Trinseo
 せん断応力-せん断速度. , CALIBRE™ MEGARAD™ 2081-15, PC, Trinseo
 pvT , CALIBRE™ MEGARAD™ 2081-15, PC, Trinseo
特殊な特性
成形加工法.
射出成形.
添加剤.
離型剤.
特殊な特性.
透明., 滅菌可能, Gamma irradiation sterilization, Electron beam (e-beam) sterilization
耐薬品性
Radiation Resistance
Certifications
Medical Grade, Biocompatibility ISO 10993
アプリケーション
医療の
領域別の利用可能性
北アメリカ., ヨーロッパ., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.